UTILIZATION OF MALAYSIAN LOW GRADE IRON ORE …
iron ore is 8%. From the graph, it can be observed that decomposition starts at temperature of 200 °C. Continuous weight loss were observed in the temperature range of 200-400 °C. The total weight loss indicates the high combine water presence in the ore. Table-1. Mineral composition of iron ore. Figure-1. Thermal analysis of original iron ...